Alloy 625
AMS 5599UNS N06625- Cr20.00–23.00
- Mo8.00–10.00
- Cb (Nb)3.15–4.15
- Fe5.00
- Co1.00
- C.10
- Mn.50
- Si.50
- Al.40
- Ti.40
- P.015
- S.015
- NiBalance
AMS & ASTM specifications for every alloy and temper we stock, with minimum mechanical properties unless otherwise noted.
Swipe sideways to see the full table →
| Alloy | Temper | Applicable Specifications | Tensilemin, psi | Yieldmin, psi | Elongationin 2″ min |
|---|---|---|---|---|---|
| 301UNS S30100EN 1.4310JIS SUS301Tech data sheetIn-stock sizes | Quarter Hard |
| 125,000 | 75,000 | 25% |
| Half Hard |
| 150,000 | 110,000 | 15% | |
| Full Hard |
| 185,000 | 140,000 | 8% | |
| 302 / 304UNS S30200 / S30400EN 1.4310 / 1.4301JIS SUS302 / SUS304Tech data sheetIn-stock sizes | Annealed |
| 75,000 | 30,000 | 40% |
| Annealed 302 / 304 is also covered by our triple-certified 304L / 304 / 302 material.Why 304L / 304 / 302? → | |||||
| Quarter Hard |
| 125,000 | 75,000 | 10% | |
| Half Hard |
| 150,000 | 110,000 | 9% | |
| Full Hard |
| 185,000 | 140,000 | 3% | |
| Our 302 / 304 material is dual certified to meet both alloys.Why 302 / 304? → | |||||
| 304LUNS S30403EN 1.4307JIS SUS304LTech data sheetIn-stock sizes | Annealed |
| 70,000 | 25,000 | 40% |
| Our 304L Annealed is triple certified to meet alloys 304L / 304 / 302.Why 304L / 304 / 302? → | |||||
| 305UNS S30500EN 1.4303JIS SUS305Tech data sheetIn-stock sizes | Annealed |
| 70,000 | 25,000 | 40% |
| 316 / 316LUNS S31600 / S31603EN 1.4401 / 1.4404JIS SUS316 / SUS316LTech data sheetIn-stock sizes | Annealed |
| 70,000 | 25,000 | 40% |
| Full Hard |
| 180,000 | 135,000 | 2% | |
| No AMS or ASTM specification sets mechanical minimums for 316 / 316L Full Hard. It is certified to the annealed specifications for chemistry only. The values shown are typical of our Full Hard material, not guaranteed minimums — actual results for your lot are reported on its certification. | |||||
| Our 316 / 316L material is dual certified to meet both alloys.Why 316 / 316L? → | |||||
| 321UNS S32100EN 1.4541JIS SUS321Tech data sheetIn-stock sizes | Annealed |
| 75,000 | 30,000 | 40% |
| 17-7PH®UNS S17700EN 1.4568JIS SUS631Tech data sheetIn-stock sizes | Annealed (Cond. A) |
| 150,000 max | 65,000 max | 20% |
| Condition C |
| 200,000 | 175,000 | 1% | |
| 410UNS S41000EN 1.4006JIS SUS410Tech data sheetIn-stock sizes | Annealed |
| 65,000–95,000 | 30,000 | 12% |
| 430UNS S43000EN 1.4016JIS SUS430Tech data sheetIn-stock sizes | Annealed |
| 65,000 | 35,000 | 20% |
| 1008 / 1010UNS G10080 / G10100Tech data sheetIn-stock sizes | #5 Temper · Annealed |
| Hardness by thickness — ASTM A109
| — | |
| #2 Temper · Half Hard |
|
| — | ||
| #1 Temper · Hard |
|
| — | ||
| Our 1008 / 1010 is certified to both alloys unless otherwise noted. ASTM A109 sets the hardness scale by thickness; values cover our range through .031″.Why 1008 / 1010? → | |||||
| Alloy 625UNS N06625EN 2.4856Tech data sheetIn-stock sizes | Annealed |
| 120,000 | 60,000 | 30% |
| C17200 Beryllium CopperUNS C17200EN CW101CRanges, not minimumsTech data sheetIn-stock sizes | TB00 (A) Annealed |
| 60,000–78,000 | 28,000–60,000 | 35–65% |
| TD01 (¼H) Quarter Hard |
| 75,000–88,000 | 60,000–80,000 | 15–40% | |
| TD02 (½H) Half Hard |
| 85,000–100,000 | 75,000–95,000 | 9–30% | |
| TD04 (H) Hard |
| 100,000–130,000 | 90,000–112,000 | 2–18% | |
| C17200 values are ranges published by NGK Metals for Berylco® 25 strip, before heat treatment. See the C17200 tech sheet for heat treated and mill hardened tempers. | |||||
Derived from applicable AMS & ASTM specifications. Always refer to the current revision of the specification.
Nearest European (EN) and Japanese (JIS) grade names for the alloys we stock, for customers who order by those designations.
For reference only. Brown Metals Company certifies to the AMS & ASTM specifications listed above — not to EN or JIS standards. Composition limits differ between systems, so these are nearest equivalents, not exact matches. Always confirm against your drawing or purchase order.
Swipe sideways to see the full table →
| Alloy | UNS | EN No. | EN Name | JIS |
|---|---|---|---|---|
| 301 | S30100 | 1.4310 | X10CrNi18-8 | SUS301 |
| 302 | S30200 | 1.4310 | X10CrNi18-8 | SUS302 |
| EN groups 301 and 302 under one grade, 1.4310. | ||||
| 304 | S30400 | 1.4301 | X5CrNi18-10 | SUS304 |
| 304L | S30403 | 1.4307 | X2CrNi18-9 | SUS304L |
| 305 | S30500 | 1.4303 | X4CrNi18-12 | SUS305 |
| 316 | S31600 | 1.4401 | X5CrNiMo17-12-2 | SUS316 |
| 316L | S31603 | 1.4404 | X2CrNiMo17-12-2 | SUS316L |
| 321 | S32100 | 1.4541 | X6CrNiTi18-10 | SUS321 |
| 17-7PH® | S17700 | 1.4568 | X7CrNiAl17-7 | SUS631 |
| 410 | S41000 | 1.4006 | X12Cr13 | SUS410 |
| 430 | S43000 | 1.4016 | X6Cr17 | SUS430 |
| Alloy 625 | N06625 | 2.4856 | NiCr22Mo9Nb | — |
| Werkstoff number (DIN), not an EN 10088 grade. | ||||
| C17200 | C17200 | CW101C | CuBe2 | — |
| EN copper alloy designation (EN 1652 / EN 1654). | ||||
EN numbers per EN 10027-2; stainless grades as listed in EN 10088. 1008 / 1010 low carbon steel has no close EN or JIS chemistry match and is not listed.
Stainless & low carbon steel — percent by weight. Maximum values unless a range or minimum is shown.
Swipe sideways to see the full table →
| Alloy | CCarbon | MnManganese | PPhosphorus | SSulfur | SiSilicon | CrChromium | NiNickel | MoMolybdenum | CuCopper | NNitrogen | TiTitanium | AlAluminum |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 301S30100 | .15 | 2.00 | .045 | .030 | .75 | 16.00– | 6.00– | .75 | .75 | .10 | — | — |
| 302S30200 | .15 | 2.00 | .045 | .030 | 1.00 | 17.00– | 8.00– | .75 | .75 | .10 | — | — |
| 304S30400 | .08 | 2.00 | .045 | .030 | 1.00 | 18.00– | 8.00– | .75 | .75 | .10 | — | — |
| Our 302 / 304 material is dual certified to meet both alloys.Why 302 / 304? → | ||||||||||||
| 304LS30403 | .03 | 2.00 | .045 | .030 | 1.00 | 18.00– | 8.00– | .75 | .75 | .10 | — | — |
| Our 304L Annealed is triple certified to meet alloys 304L / 304 / 302.Why 304L / 304 / 302? → | ||||||||||||
| 305S30500 | .12 | 2.00 | .045 | .030 | 1.00 | 17.00– | 10.50– | .75 | .75 | .10 | — | — |
| 316S31600 | .08 | 2.00 | .040 | .030 | 1.00 | 16.00– | 10.00– | 2.00– | .75 | — | — | — |
| 316LS31603 | .03 | 2.00 | .040 | .030 | 1.00 | 16.00– | 10.00– | 2.00– | .75 | — | — | — |
| Our 316 / 316L material is dual certified to meet both alloys.Why 316 / 316L? → | ||||||||||||
| 321S32100 | .08 | 2.00 | .045 | .030 | .75 | 17.00– | 9.00– | .75 | .75 | .10 | 5×(C+N) min – | — |
| 17-7PH®S17700 | .09 | 1.00 | .040 | .030 | 1.00 | 16.00– | 6.50– | — | — | — | — | .75– |
| 410S41000 | .08– | 1.00 | .040 | .030 | 1.00 | 11.50– | — | — | — | — | — | — |
| 430S43000 | .12 | 1.00 | .040 | .030 | 1.00 | 16.00– | .75 | — | — | — | — | — |
| 1008 / 1010G10080 / G10100 | .08– | .30– | .025 | .025 | — | .15 | .20 | .06 | .20 | — | — | — |
| Our 1008 / 1010 is certified to both alloys — the carbon range shown is the window that meets both.Why 1008 / 1010? → | ||||||||||||
Derived from applicable AMS & ASTM specifications. Hover a column to highlight it.
Percent by weight, maximum unless a range or minimum is shown.
Superseded military, federal and ASTM specifications mapped to their current AMS or ASTM replacements.
Swipe sideways to see the full table →
| Cancelled Spec | Alloy | Temper / Grade | Replacement |
|---|---|---|---|
| MIL-S-5059 | 301 | Annealed | AMS 5901 |
| ¼ Hard | AMS 5517 | ||
| ½ Hard | AMS 5518 | ||
| ¾ Hard | AMS 5902 | ||
| Full Hard | AMS 5519 | ||
| MIL-S-5059 | 302 | Annealed | AMS 5516 |
| ¼ Hard | AMS 5903 | ||
| ½ Hard | AMS 5904 | ||
| ¾ Hard | AMS 5905 | ||
| Full Hard | AMS 5906 | ||
| MIL-S-5059 | 304 | Annealed | AMS 5513 |
| ¼ Hard | AMS 5910 | ||
| ½ Hard | AMS 5911 | ||
| ¾ Hard | AMS 5912 | ||
| Full Hard | AMS 5913 | ||
| MIL-S-5059 | 316 | Annealed | AMS 5524 |
| ¼ Hard | AMS 5907 | ||
| QQ-S-766 | Stainless | Cold worked grades | ASTM A666 |
| Precipitation hardening grades | ASTM A693 | ||
| All other grades | ASTM A240 | ||
| MIL-S-25043 | 17-7PH® | Annealed | AMS 5528 |
| Condition C | AMS 5529 | ||
| ASTM A167 | Stainless | Grades covered by both A167 and A240 | ASTM A240 |
| Grades previously covered in both ASTM A167 and ASTM A240 have been removed from A167 and transferred to A240. | |||
| QQ-S-698 | 1008 / 1010 | All tempers | ASTM A109 |
Educational information only — always order to the current revision of the governing specification.